Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding 33% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Oxford Polymers Oxnilon 66-33GF 33% Glass Fiber Filled Nylon 66 for Injection Molding 33% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | |
Pacific Sintered Materials F-241-T Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-20All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | |
Pacific Sintered Materials FN-250-S Nickel Iron Powdered Metal Good impact resistant mechanical components. Good hardenability.Equivalent MPIF Specification: FN-0200-20All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | |
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-20Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | 0.125 in; ASTM D638 |
Matrixx Group 80S7451 45% Glass Reinforced PET
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |
|||
Tensile Strength, Yield | 172 MPa @Thickness 6.35 mm |
25000 psi @Thickness 0.250 in |
LW |
Industrial Laminates/Norplex MC603 Paper Base Laminate
(discontinued **) Description: MC603 is constructed from electrical grade of kraft paper and a specially modified phenolic resin system, and is designed to be used in tap changers, coil support plates and terminal pa.. |
|||
Tensile Strength, Yield | 172 - 310 MPa @Strain 0.200 % |
25000 - 45000 psi @Strain 0.200 % |
|
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper A(TB00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Tensile Strength, Yield | 172 - 310 MPa @Strain 0.200 % |
25000 - 45000 psi @Strain 0.200 % |
|
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | .01% permanent set |
Meehanite GM-60 Flake Graphite Cast Iron Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF34 IM HS 34% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 34% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF35 LE 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant Features: Lubricated and Low ExtractablesInformation provided by TP .. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 IM L NAT002 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | Annealed |
Special Metals MONEL® 404 Copper-Nickel Alloy Data provided by California Fine Wire and the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 BK 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 RM L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Low Moisture Absorption and.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 SL5 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Silicone Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES HiFill® PPA GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 GF40 ML2 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Heat Stabiliz.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 GF43 ML2 BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 43% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated Appearance: BlackTPCI# 8047101Informa.. |
|||
Tensile Strength, Yield | 172 MPa @Strain 0.200 % |
25000 psi @Strain 0.200 % |
|
Universal Wire Works Commercially Pure (AMS 4951) Titanium Alloy Filler Metal Universal commercially pure titanium is extremely versatile for applications requiring high temperature resistance together with resistance to many chemical reagents. Commercially pure (cp) titanium.. |
|||
Tensile Strength, Yield | >= 172 MPa | >= 25000 psi | 0.2% Offset |
Eagle Brass 305 Austenitic Stainless Steel, Annealed Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
Tensile Strength, Yield | >= 172 MPa | >= 25000 psi | 0.2% Offset |
Eagle Brass 316L Austenitic Stainless Steel, Annealed Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Tensile Strength, Yield | 172 - 455 MPa | 25000 - 66000 psi | |
Chicago Extruded Metals BioBrass® UNS C46400 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, wire, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Met.. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Clariant PA612G30 Nylon 612, 30% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Clariant PA621G30 Nylon 612, 30% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Clariant Renol PA211G40 Nylon 6, 40% Glass Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | Annealed |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 172 MPa | 25000 psi | ASTM D638 |
Asahi Kasei Thermylon® NSG-730A 65% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |