Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.2 MPa | 3950 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CR120CL-01 Polypropylene, Random Copolymer, Clarified COPYLENE™ CR120CL-01 is a clarified, random copolymer specially designed for injection molding applications and is formulated with anti-stat for excellent mold release.Applications: Injection moldi.. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-NP-110-W-NAT Polyamide 12 (Nylon 12) Information provided by PolyOne |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | aged 70 hours at 250ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | 50 mm/min. Type IV; ASTM D638 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | ASTM D-882 |
Saint-Gobain Norton® F510 General Purpose Skived PTFE Sheet Description: PTFE = polytetrafluoroethyleneApplications include: General Purpose; Common in Electrical/ElectronicsInformation provided by Saint Gobain Performance Products. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | ASTM D638 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | ASTM D638 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | ASTM D638 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | ASTM D638 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | ASTM D638 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | ASTM D638 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | aged 70 hours at 250ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 27.2 MPa | 3950 psi | ASTM D638 |
Dow C759-21NA Polypropylene Impact Copolymer Resin DOW C759-21NA Polypropylene Resin is an impact copolymer designed for injection molding with high stiffness, good impact resistance, and good antistatic properties. Key applications include foldabl.. |