Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.00 MPa
290 psi
Conductive Layer
Fujipoly Industries Zebra® Silver Connector
Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive laye..
Tensile Strength, Yield >= 2.00 MPa
>= 290 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7075 Ethylene-Propylene Rubber
General service EPDM.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 2.00 MPa
290 psi
ISO 527
Styrolution Styrolux S SBC
Styrolux S is a new developmental, clear styrene-butadiene copolymer (SBC) designed specifically for blending with Styrolux T in order to enable high performance film extrusion and shrink film appli..
Tensile Strength, Yield 2.00 MPa

@Strain 100 %
290 psi

@Strain 100 %
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content
Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries.
Tensile Strength, Yield 2.00 MPa
290 psi
508 mm/min; ASTM D638
Dow Engage® 8400 Polyolefin Elastomer
Description: Engage® 8400 and Engage® 8407 polyolefin elastomers are ethylene-octene copolymers that offer excellent performance in durable injection molded industrial and consumer goods and compr..
Tensile Strength, Yield 2.00 MPa
290 psi
508 mm/min; ASTM D638
Dow Engage® 8407 Polyolefin Elastomer
Description: Engage® 8407 polyolefin elastomer is an ethyleneoctene copolymer with a nominal loose talc coating. The talc is untreated and has a 1µm particle size. Engage® 8407 offers excellent p..
Tensile Strength, Yield 2.00 MPa
290 psi
ACC MM906 Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing..
Tensile Strength, Yield 2.00 MPa
290 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® IT 36-018 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerGood Surface AppearanceOpaqueApplications:AutomotiveInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by P..
Tensile Strength, Yield 2.00 MPa
290 psi
ASTM D3574
Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..
Tensile Strength, Yield 2.00 MPa

@Strain 100 %
290 psi

@Strain 100 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® ST-6350 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Over-Molding GradeApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.