Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 172 - 310 MPa @Strain 0.200 % |
25000 - 45000 psi @Strain 0.200 % |
|
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper A(TB00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Tensile Strength, Yield | 170 - 310 MPa @Strain 0.200 % |
24700 - 45000 psi @Strain 0.200 % |
|
Kobe Steel KS40 Commercially Pure Titanium, ASTM Gr. 1, Annealed Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel |
|||
Tensile Strength, Yield | 170 - 310 MPa | 24700 - 45000 psi | 0.2% proof |
Kobe Steel KS40PDA Titanium alloy with low alloying elements, ASTM Gr. 11, Annealed Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by .. |
|||
Tensile Strength, Yield | 170 - 310 MPa @Strain 0.200 % |
24700 - 45000 psi @Strain 0.200 % |
|
Kobe Steel KS40S Commercially Pure Titanium, ASTM Gr. 1, Annealed Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel |
|||
Tensile Strength, Yield | 172 - 310 MPa @Strain 0.200 % |
25000 - 45000 psi @Strain 0.200 % |
|
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 241 - 310 MPa @Temperature 20.0 °C |
35000 - 45000 psi @Temperature 68.0 °F |
typical |
H.C. Starck Ultra 76 Alloy (Ta 2.5%W) Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low.. |
|||
Tensile Strength, Yield | 103 - 310 MPa | 15000 - 45000 psi | |
Chicago Extruded Metals UNS C36000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 103 - 310 MPa | 15000 - 45000 psi | |
Chicago Extruded Metals UNS C36010 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 138 - 310 MPa @Strain 0.200 % |
20000 - 45000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899L Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 138 - 310 MPa @Strain 0.200 % |
20000 - 45000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899M Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 138 - 310 MPa @Strain 0.200 % |
20000 - 45000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |