Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.6 MPa | 3130 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable MAF110A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | ASTM D638 |
PolyMirae Moplen RP210R Extrusion Coating and Lamination Grade Polypropylene Moplen RP210R is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP210R is a copolymer particularly suitable for extrusion coating and.. |
|||
Tensile Strength, Yield | 21.6 - 23.5 MPa | 3130 - 3410 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Tensile Strength, Yield | 21.6 - 23.5 MPa | 3130 - 3410 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | ASTM D638 |
I. Stern HIPS SH03 High Impact Polystyrene Features:High flowExcellent toughnessExcellent processabilityApplicationsInjection moldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co. Inc. |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | 50 mm/min; ASTM D638 |
LG Chemical SEETEC PH150 HDPE Blown Film Grade Features: Characteristics : Excellent weather resistance & Environmental stress cracking resistanceAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 20.. |
|||
Tensile Strength, Yield | 21.6 MPa @Thickness 3.20 mm |
3130 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HM5302W PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | ISO 527-2 |
Styron DGF080.00 ESU Polypropylene Overview: 10% glass filled polypropyleneNaturalMedium flowHeat ResistantInformation provided by Styron |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S160D Thermoplastic Polyurethane Type: Estane® S160D is a Shore 63D, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S360D Thermoplastic Polyurethane Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 2575N injection Molded Polypropylene Impact Copolymer for High Speed injection Molded ApplicationsFormolene® 2575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging, .. |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | ASTM D638 |
Westlake Plastics Lennite® SD-P UHMW-PE (static dissipative) Carbon-powder filled, self-lubricating, moisture-repellent material with resistivity levels in the 10^5-10^9 range. This material has the highest impact strength, is lightweight, has excellent abra.. |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | |
Zylog Hipolyene® 3080 HC RM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | |
Zylog Hipolyene® 5131 SX-5 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 21.6 MPa | 3130 psi | |
Zylog Hipolyene® 8021 T Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |