Tensile Strength, Yield 33.1 MPa
4800 psi
2 in per min; ASTM D638
Network Polymers NPP 30-1200
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Tensile Strength, Yield 33.1 MPa
4800 psi
2 in/min; ASTM D638
Phillips 66 COPYLENE® CH020 Polypropylene, Homopolymer, BOPP
COPYLENE™ CH020 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches; Raffia/Tapes/Strapping; Peelable..
Tensile Strength, Yield 33.1 MPa
4800 psi
(2 in/min); ASTM D638
Phillips 66 COPYLENE® CH020-03 Polypropylene, Homopolymer, BOPP
COPYLENE™ CH020-03 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applicationsApplications: Bags & Pouches, Raffia/Tapes/Strapping, Peelabl..
Tensile Strength, Yield 33.1 MPa
4800 psi
(2 in/min); ASTM D638
Phillips 66 COPYLENE® CH020S Polypropylene, Homopolymer, BOPP
COPYLENE™ CH020S is a polypropylene homopolymer resin typically used by customers for BOPP (biaxially oriented polypropylene) Applications: Film ExtrusionInformation provided by Phillips 66.
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
M. Holland Company PP100 Polypropylene Homopolymer, General Purpose
High clarityHomopolymerGood melt strengthHigh tensile strengthApplications: Thin-walled partsSheetStrapping
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Ineos N00N-00 Polypropylene Impact Copolymer
Grade N00N-00 is a fractional melt flow rate, high impact copolymer polypropylene specifically designed for non-pressure structured wall pipe but can also be used in other extrusion applications req..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
LTL Color Compounds ColorRxâ„¢ PP1-2000RX Biocompatible Polypropylene Homopolymer
A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications.All information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
LTL Color Compounds ColorRxâ„¢ PP1-2002AF Food Grade Polypropylene Homopolymer
A 20 melt injection molding grade of Polypropylene homopolymer with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
LTL Color Compounds ColorRxâ„¢ PP1-2005ARX Biocompatible Polypropylene Homopolymer
A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All in..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Ineos N01N-00 Polypropylene Impact Copolymer
Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properti..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Techmer ES HiFill® HDPE MM40 40% Mica Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mica Filler, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Spartech Royalite R21 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Techmer ES HiFill® PP 0096 S2 LE Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Techmer ES Plastiblend® ABS IM
Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene
DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin
Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPallets..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene
DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m..
Tensile Strength, Yield 33.1 MPa
4800 psi
2" (50mm) per min.; ASTM D638
Formosa Plastics Formolene® 5102KR Cast Film Polypropylene
HomopolymerApplications: Biaxially oriented film.Formolene 5102KR is a highly isotactic polypropylene homopolymer designed primarily for cast film applications such as slit tape fabric stock and cor..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene
DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Eastman Tenite 105E3V36327 Acetate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Dow H700-12 Polypropylene Homopolymer Resin
Complies withU.S. FDA 21 CFR 177.1520 (c) 1.1FDA-DMFUnderwriters Laboratories Inc.Europe EU-Directive 2002/72/ECLondon Metal Exchange - Part 6B Rules - PolypropyleneCanadian HPFB No ObjectionDOW H70..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D412
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea
RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This ne..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D-638
Bapolene® 4072 Polypropylene, Injection Grade
Bapolene PP4072 is a high flow, fast cycle injection molding resin. This product meets FDA standards for food contact applications.Applications: Appliances, containers, and thin-walled articles.Bap..
Tensile Strength, Yield 33.1 MPa
4800 psi
Asahi Kasei Thermylene® P-20TC-1156 Chemically Coupled Polypropylene Compound, 20% Talc Filled
Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei
Tensile Strength, Yield 33.1 MPa
4800 psi
50 mm/min; ASTM D638
Amco PRIMATOP PP HOMO 011 Extrusion Processing Polypropylene
PP HOMO 011 features high molecular weight, high isotactic, and does not contain slip or anti-block. Applications include strapping, various extrusion profile, and sheet and film applications.Former..
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Birch Plastics RPP1215 Recycled Polypropylene
RPP1215 is a homopolymer polypropylene reprocessed pellets made from 100% post industrial recycled material made for injection molding applications.Information provided by Birch Plastics, Inc.
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Copyright © lookpolymers.com All Rights Reserved