Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 359 MPa @Temperature 71.1 °C |
52000 psi @Temperature 160 °F |
0° Direction, Wet; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 359 MPa | 52000 psi | |
Performance Alloys MoldStar® 18 (PAS 18) Bronze Mold Alloy Description: MoldStar® 18 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: SlidesGibsWear PlatesMold Locking DevicesSl.. |
|||
Tensile Strength, Yield | 359 MPa @Strain 0.200 %, Temperature 260 °C |
52100 psi @Strain 0.200 %, Temperature 500 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 359 MPa @Strain 0.200 %, Temperature 204 °C |
52100 psi @Strain 0.200 %, Temperature 399 °F |
|
Haynes Ultimet® alloy, 12.7-50.8 mm bar Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 359 MPa @Strain 0.200 % |
52100 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 359 MPa @Strain 0.200 % |
52100 psi @Strain 0.200 % |
|
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Round 1.500 in (38.1 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 1.500 inch round. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Tensile Strength, Yield | >= 359 MPa | >= 52100 psi | |
Alcoa Excalibar® 6013-T651 Aluminum Alcoa recommends as a higher machinability alternative to 6061-T651. It has the potential for higher machining speeds and feed rates, easier deburring,ease of clearing 'chips' and better finishes. .. |
|||
Tensile Strength, Yield | 359 MPa | 52000 psi | |
AK Steel DI-MAX® M-15 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |