Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 345 - 414 MPa @Strain 0.200 % |
50000 - 60000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 345 - 414 MPa @Strain 0.200 % |
50000 - 60000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 207 - 414 MPa @Strain 0.200 % |
30000 - 60000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann.. |
|||
Tensile Strength, Yield | 241 - 414 MPa @Strain 0.200 % |
35000 - 60000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3.. |
|||
Tensile Strength, Yield | 352 - 414 MPa | 51000 - 60000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, 3/4 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | 290 - 414 MPa | 42000 - 60000 psi | 0.2% offset |
Eagle Brass 260 Cartridge Brass, 1/2 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Yield | 103 - 414 MPa | 15000 - 60000 psi | 0.2% offset |
Eagle Brass 735 Nickel Silver 18%, Annealed 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |