Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 290 - 365 MPa | 42000 - 53000 psi | 0.2% offset |
Eagle Brass 220 Commercial Bronze, 1/2 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Yield | 290 - 414 MPa | 42000 - 60000 psi | 0.2% offset |
Eagle Brass 260 Cartridge Brass, 1/2 Hard Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul.. |
|||
Tensile Strength, Yield | 290 - 483 MPa | 42000 - 70000 psi | 0.2% offset |
Eagle Brass 511 Phosphor Bronzes 4%, 1/2 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Yield | 290 - 448 MPa | 42000 - 65000 psi | 0.2% offset |
Eagle Brass 706 Copper Nickel 10%, 1/4 Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Tensile Strength, Yield | 290 MPa | 42000 psi | |
AK Steel DI-MAX® M-36 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |