Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 29.0 MPa | >= 4210 psi | ASTM D638 |
NIZHNEKAMSKNEFTEKHIM PP 4310M (EP1X30F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50 mm/min; ASTM D638 |
NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersIn.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50 mm/min |
Polimeri Europa EDISTIR RK0414 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-03-04-23 UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded high impact polystyrene with excellent light .. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Global V-1160 High Density Polyethylene, Injection Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in.. |
|||
Tensile Strength, Yield | 29.0 - 68.9 MPa | 4210 - 10000 psi | Average value: 32.2 MPa Grade Count:17 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Flint Hills P6G2N-095 Impact Copolymer Polypropylene Features: Excellent stiffness and impact resistance, nucleated, suitable for retort and hot fill applications. Product does not contain animal derived components.Applications: Blow molding, sheet/.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ISO 527 |
GEHR Plastics PE-ELS® Polyethylene HDPE A variant of PE-HD with improved electrical conductivity.Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties a.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638-02 |
Ipiranga Petrochem HA 7260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | cond.; ISO 527-1, -2; 50 mm/min |
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
LyondellBasell Astryn 65F4-4 Polypropylene Homopolymer, 40% Talc Key Features: conventional melt flow, high modulus, mineral-filled polypropylene homopolymer, high stiffness, good dimensional stability, excellent heat resistanceApplications: automotive heater and.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50mm/min; ISO 527-2 |
Borealis Borclear™ RF366MO Polypropylene Random Copolymer for Injection Molding Borclear™ RF366MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is designed for high-speed injection molding and contains nucleati.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene DescriptionPolyfort® FPP 1237 is a 20% CAC03 filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50mm/min; ISO 527-2 |
Borealis RF365MO Polypropylene Applications: closures, thin wall containers, and excellent transparency.Information provided by Borealis AG |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ISO 527 |
Total HDPE HD 6081 High Density Polyethylene - Injection Molding HD 6081 is a high density polyethylene with very good organoleptic properties, rigidity and processability.It is especially suited for the production of caps & closures for non-carbonated drinks by .. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ISO 527 |
Total Lumicene® M6040 Metallocene High Density Polyethylene Lumicene® M6040 is a second generation metallocene high density polyethylene with very good organoleptic properties, dimensional stability, rigidity and processability.It is especially suited for t.. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 2 in/min; ASTM D638 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 2 in/min, Type IV bar; ASTM D638 |
Chevron Phillips Marlex® K605 HDPE Blow Molding Resin Resin Type: Ethylene HomopolymerCharacteristics: Good ESCRExceptional rigidityExcellent melt strengthApplications: Automotive bumper beamsInformation provided by Chevron Phillips. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Entec Hypro™ PPC-T10 Copolymer Polypropylene, 10% Talc Reinforced Information provided by Entec |
|||
Tensile Strength, Yield | 29.0 MPa @Temperature 23.0 °C |
4210 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FN714 NC010A Nylon 66 Zytel® FN714 NC010A is an impact modified, very flexible, plasticizer free polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ISO 527 |
Eurostar Starpylen HZ 30WF2 PP, 30% Wood Fiber Filled, Injection Molding Starpylen HZ 30WF2 is a 30% Wood Fiber Reinforced Polypropylene Injection Molding Resin (also known as HZ30WF2)Information provided by Eurostar. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334C30L Calcium Reinforced |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | |
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | |
BASF Novolen® 3248 RC Polypropylene Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM-D638 |
Polyram RamOfin PPC359T4 Polypropylene, 20% Mineral Filled 20% mineral filled, heat stabilized and impact modified for polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 29.0 MPa | 4210 psi | ASTM-D638 |
Braskem HB0454 HDPE Blow Molding Polyethylene Copolymer HB0454 is a high-density polyethylene copolymer resin with average molecular weight produced by the Unipol® process. A bottle made with HB0454 shows excellent processability, color, and superficial.. |