Mechanical Properties Metric English Comments
Tensile Strength, Yield 172 - 310 MPa

@Strain 0.200 %
25000 - 45000 psi

@Strain 0.200 %
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper A(TB00)
C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated..
Tensile Strength, Yield 170 - 310 MPa

@Strain 0.200 %
24700 - 45000 psi

@Strain 0.200 %
Kobe Steel KS40 Commercially Pure Titanium, ASTM Gr. 1, Annealed
Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel
Tensile Strength, Yield 170 - 310 MPa
24700 - 45000 psi
0.2% proof
Kobe Steel KS40PDA Titanium alloy with low alloying elements, ASTM Gr. 11, Annealed
Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by ..
Tensile Strength, Yield 170 - 310 MPa

@Strain 0.200 %
24700 - 45000 psi

@Strain 0.200 %
Kobe Steel KS40S Commercially Pure Titanium, ASTM Gr. 1, Annealed
Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel
Tensile Strength, Yield 172 - 310 MPa

@Strain 0.200 %
25000 - 45000 psi

@Strain 0.200 %
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast)
Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr..
Tensile Strength, Yield 241 - 310 MPa

@Temperature 20.0 °C
35000 - 45000 psi

@Temperature 68.0 °F
typical
H.C. Starck Ultra 76 Alloy (Ta 2.5%W)
Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low..
Tensile Strength, Yield 103 - 310 MPa
15000 - 45000 psi
Chicago Extruded Metals UNS C36000 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Tensile Strength, Yield 103 - 310 MPa
15000 - 45000 psi
Chicago Extruded Metals UNS C36010 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Tensile Strength, Yield 138 - 310 MPa

@Strain 0.200 %
20000 - 45000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899L Skin Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 138 - 310 MPa

@Strain 0.200 %
20000 - 45000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899M Skin Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 138 - 310 MPa

@Strain 0.200 %
20000 - 45000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899A Skin Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..