Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 414 - 483 MPa @Strain 0.200 % |
60000 - 70000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 414 - 483 MPa @Strain 0.200 % |
60000 - 70000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 276 - 483 MPa | 40000 - 70100 psi | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Tensile Strength, Yield | 372 - 483 MPa | 54000 - 70000 psi | 0.2% offset |
Eagle Brass 18665 MSP1, 1/2 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Yield | 400 - 483 MPa | 58000 - 70000 psi | 0.2% offset |
Eagle Brass 19210 XP-10 Copper Iron, Extra Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Yield | 400 - 483 MPa | 58000 - 70000 psi | 0.2% offset |
Eagle Brass 425 Tin Brass 2%, 3/4 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Yield | 290 - 483 MPa | 42000 - 70000 psi | 0.2% offset |
Eagle Brass 511 Phosphor Bronzes 4%, 1/2 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Yield | 379 - 483 MPa | 55000 - 70000 psi | 0.2% offset |
Eagle Brass 519 Phosphor Bronzes 6%, 1/2 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Strength, Yield | 241 - 483 MPa | 35000 - 70000 psi | 0.2% offset |
Eagle Brass 762 Nickel Silver 12%, 1/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |