Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 34.5 MPa | 5000 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 30-0400 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 34.5 MPa @Thickness 3.20 mm |
5000 psi @Thickness 0.126 in |
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 1220 Polypropylene Homopolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 34.5 MPa @Thickness 3.20 mm |
5000 psi @Thickness 0.126 in |
At 51mm/min, thick injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 1517 Polypropylene Homopolymer, Fiber Spinning Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 34.5 - 76.0 MPa | 5000 - 11000 psi | Average value: 51.4 MPa Grade Count:46 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | Coatings catalyzed 2% with 9995, baked 15 minutes @ 107ºC, post cured 2 weeks @ 25ºC and 50% relative humidity. Free films tested on an Instron tester |
Lord Adhesives Chemglaze® V004 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Spartech Weather-Pro Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D 638 |
Styrolution PS 1900 GPPS Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Tipco Tipcolene® FPT 20 - 20% Talc Reinforced Polypropylene Homopolymer Compound 20% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Washington Penn Homopolymer Polypropylene 30% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 5144H Homopolymer Polypropylene Homopolymer for Appliance Applications Formolene® 5144H is a highly isotactic polypropylene homopolymer designed for consumer products and appliance applications requiring long-term heat-aging res.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3488-01 is a specially formulated homopolymer polypropylene designed for large appliance injection molding. This material has excellent chemical resistance in addition t.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 3489-01 Polypropylene Homopolymer DescriptionPolypropylene PP 3489-01 is a specially designed homopolymer with excellent stiffness properties. ApplicationTypical applications include high speed extrusion, high speed thin wall injec.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP30-0500 Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM Data |
Dow H700-12 Polypropylene Homopolymer Dow Polypropylene Homopolymer Resins are semi-crystalline thermoplastic materials that can provide a combination of desirable properties and affordability: low density; excellent chemical resistance.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Engineered Polymer Solutions ABS PCR 400, Recycled General Purpose with 40% Post Consumer ABS. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Asahi Kasei Thermofil P-9900-0712 Unfilled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Aaron Industries AAROLENE® AVPS HIPS 100-3 MELT 14 Virgin HIPS Resin A virgin, high impact polystyrene, natural in color, specifically designed for injection molding applications. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 34.5 MPa | 5000 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 1102KR Cast Film Polypropylene HomopolymerApplications: Cast film applications such as slit tape fabric stock and cordage.Formolene 1102KR is a highly isotactic polypropylene homopolymer designed primarily for cast film applicati.. |