Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
PTS Trilac® ABS-HH2000 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2040MHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
PTS Trilac® ABS-HF5500 High Flow ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 51.7 - 88.3 MPa | 7500 - 12800 psi | Average value: 65.7 MPa Grade Count:3 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D-638 |
Glastic 1125 Corrosion-Resistant Panels Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1125 is asbestos-fr.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Global NPP-130-C Glass/Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PCT1000 PC/PET Alloy PC/PET alloy with outstanding chemical resistance and impact strengthAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 IM 511 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 FR NAT Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 FR IM HS BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill® PA6 0303 B Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityAppearance: Natural Color and WhiteInformation provided by TP Composites, Inc... |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Star Plastics PC/PBT7820 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill® POM CO GC20 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill® POM HO 0167 S1 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: HomopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM 638 |
PlastxWorld CEVIAN®-V 510 ABS High Modulus ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | |
TriStar TriSteel AC Metal Backed PTFE Bearing System Ultraflon 601 (AC) POM lined metal backed bearing system, boundary lubrication required, high PV. Ultraflon 601 POM Liner is a lubricant enhanced acetal material for use in lubricated or unlubricate.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | |
TriStar TriSteel AT Metal Backed PTFE Bearing System Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM 638 |
PlastxWorld CEVIAN® B14E0 PBT/ABS Alloy Excellent flowability, high impact strength and toughness. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC) Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical re.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 1000 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Clariant Renol 612-01L Nylon 612, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FM-Y249B 30% Glass/Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-5GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | Type I, 51 mm/min; ASTM D638 |
Styron PULSE™ EXT 100 PC/ABS Engineering Resin Overview: PULSE EXT 100 engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT 100 engin.. |