Polymer Property : Tensile Strength, Yield = 5120 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
PolyMirae Moplen EP340G Sheet and Thermoforming Grade Polypropylene
Moplen RP340G is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340G is a random copolymer particularly suitable for..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
PolyMirae Moplen EP340K Sheet and Thermoforming Grade Polypropylene
Moplen RP340K is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340K is a random copolymer particularly suitable for..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
PolyMirae Moplen HP524J BDDP Film Grade Polypropylene
Moplen HP524J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP524J is a homopolymer particularly suitable for BOPP (Tender) fil..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
PolyMirae Moplen HP550K Stretch/Yarn, Monofilament Grade Polypropylene
Moplen HP550K is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP550K is a homopolymer suitable for rope, tape, yarn, monofilament..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
PolyMirae Moplen HP600N Injection Molding Grade Polypropylene
Moplen HP600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600N is a homopolymer particularly suitable for injection molding..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
PolyMirae Moplen RP370G Blow Molding Grade Polypropylene
Moplen RP370G is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP370G is a copolymer particularly suitable for blow molding applicat..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
PolyMirae Moplen HP521M IPP/WQBF Grade Polypropylene
Moplen HP521M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP521M is suitable for core resin of co-extrusion CPP film. Moplen ..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Hyosung Topilene B200 PP
B200 Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:StiffnessFormabilityInformation provided by Hyosung Corporation
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Hyosung Topilene B200P PP
B200P Applications: Industrial pipesCharacteristics: Chemical resistanceInformation provided by Hyosung Corporation
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Hyosung Topilene B201Y PP
B201Y Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:Low smellFormabilityInformation provided by Hyosung Corporation
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Hyosung Topilene F301U PP
F301U Extrusion General HomopolymerApplications: Heavy duty bagCharacteristics:ProcessabilityWeatherabilityHigh tenacityInformation provided by Hyosung Corporation
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Hyosung Topilene F400 PP
F400 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Hyosung Topilene F501 PP
F501 Extrusion General HomopolymerApplications:Flat yarnRopeBandCharacteristics:ProcessabilityInformation provided by Hyosung Corporation
Tensile Strength, Yield 35.3 MPa

@Thickness 3.20 mm
5120 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical ALPHALAC SG970 HIPS
Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical
Tensile Strength, Yield 35.3 MPa

@Thickness 3.20 mm
5120 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical SH610S ABS, Excellent Surface, High Impact
Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Lotte Chemical Titan TITANPRO® 6331 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Lotte Chemical Titan TITANPRO® 6431 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Lotte Chemical Titan TITANPRO® 6531M Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Lotte Chemical Titan TITANPRO® PM655 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Tensile Strength, Yield 35.3 MPa

@Thickness 3.20 mm
5120 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical ALPHALAC SG970NSU HIPS
Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by..
Tensile Strength, Yield 35.3 MPa
5120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR
Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus..
Tensile Strength, Yield 35.3 MPa
5120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR
Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 35.3 MPa
5120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR
Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus..
Tensile Strength, Yield 35.3 MPa
5120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR
Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 35.3 MPa
5120 psi
at 300% elongation; ASTM D412
Lubrizol Estane® S360D Thermoplastic Polyurethane
Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..
Tensile Strength, Yield 35.3 MPa
5120 psi
2 in/min; ASTM D638
ExxonMobil PP1024E4 Homopolymer
Product Description: Medium melt flow rate homopolymer. Particularly suitable for general purpose injection moldingAvailability: North America Features:Autoclave SterilizableEthylene Oxide Steriliz..
Tensile Strength, Yield 35.3 MPa
5120 psi
2.0 in/min; ASTM D638
ExxonMobil Exxtral™ MDK340 Performance Polyolefin
Product Description: A medium melt flow rate, 40% mineral-filled polyolefin resin suitable for injection molded consumer products and appliance applications requiring long-term heat ageing resistanc..