Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Omni Plastics OmniTech™ ABS GRC10 NA Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond.. |
|||
Tensile Strength, Yield | 55.8 MPa @Temperature 23.0 °C |
8090 psi @Temperature 73.4 °F |
ASTM D638 |
PolyOne Geon™ CPVC MC250 Polyvinyl Chloride, Chlorinated (CPVC) The Geon MC250 CPVC is an injection molding fittings compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geo.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8090 psi | ASTM D638 |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 55.8 - 172 MPa | 8100 - 24900 psi | Average value: 79.1 MPa Grade Count:46 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/66 IM 6040 MB Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES Electrablend® PC/ABS Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES Electrablend® PC/ABS 033009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 FR 344 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES HiFill® HDPE GF30 A1 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES Luriblend® PA6 TL25 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (25%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.8 MPa | 8090 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ IM 401-11 Polycarbonate Resin Overview: CALIBREâ„¢ IM 401-11 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4410-11 MFR Polycarbonate EMERGEâ„¢ PC 4410-11 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8090 psi | ASTM Data |
Styron CALIBRE™ IM 401 11 Polycarbonate, Impact Modified CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM401 polycarbonate resins exhibit an excellent balance of impact strength and.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Styron CALIBREâ„¢ IM 401-11 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D-638 |
Axiall ProTherm® 4510 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4510 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high che.. |
|||
Tensile Strength, Yield | 55.8 MPa @Temperature 649 °C |
8090 psi @Temperature 1200 °F |
|
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc.. |
|||
Tensile Strength, Yield | 55.8 - 145 MPa | 8100 - 21000 psi | Average value: 83.2 MPa Grade Count:10 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8100 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 FR 344 BK Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |