Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 380 - 550 MPa @Strain 0.200 % |
55100 - 79800 psi @Strain 0.200 % |
|
Kobe Steel KS70 Commercially Pure Titanium, ASTM Gr. 3, Annealed Nominal Composition: Ti-Fe-OApplications: Tube sheets.Features: Relatively high strength, excellent corrosion resistance.Information provided by Kobe Steel |
|||
Tensile Strength, Yield | 380 MPa | 55100 psi | |
MMCC Aluminum/Al2O3 55p Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
MetalTek H 188 Centri-Vac Nickel Cobalt Based Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 % |
55100 psi @Strain 0.200 % |
|
Haynes 230® alloy, plate, 4000 hours exposure at 760°C (1400°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 % |
55100 psi @Strain 0.200 % |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Tensile Strength, Yield | 380 - 590 MPa | 55100 - 85600 psi | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 % |
55100 psi @Strain 0.200 % |
|
Haynes 556® alloy, 10% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 %, Temperature 95.0 °C |
55100 psi @Strain 0.200 %, Temperature 203 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 %, Temperature 550 °C |
55100 psi @Strain 0.200 %, Temperature 1020 °F |
Precipitation Hardened prior to test |
Special Metals NIMONIC® Alloy PE16 A precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. It has good strength and oxidation resistance at temperatures to about 1380°.. |
|||
Tensile Strength, Yield | 380 - 450 MPa @Strain 0.200 % |
55100 - 65300 psi @Strain 0.200 % |
|
SSAB Tunnplat Aluzink 380A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Tensile Strength, Yield | 380 MPa | 55100 psi | |
SSAB Tunnplat Domex® 044 BOR Rolled Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
ThyssenKrupp PAS 380 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Not listed in the ASTM.Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
AK Steel ASTM A 1011, Grade 55 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
AK Steel ASTM A 570, Grade 55 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
AK Steel ASTM A 607 Class 2 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Yield | 380 MPa | 55100 psi | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367) The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
AK Steel ASTM A 1011, Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 380 MPa | >= 55100 psi | |
AK Steel SAE J1392, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 % |
55100 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 15-7 High Strength Stainless Steel, UNS S15700 Property data below is typical of annealed samples. Available in sheet and strip. For use in high-strength springs, bellows, and aerospace applications.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 380 - 450 MPa | 55100 - 65300 psi | |
ArcelorMittal HSLA 380 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC380LA), electroglavanized (HC380LA +ZE) and Extragal®/galfan/Galvannealed (HC380LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |