Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 % |
>= 80000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys WNF-2109 Tungsten Heavy Alloy Mil. T-21014 Class 4, SAE-AMS-T-21014 Class 4, ASTM-B-777-87 Class 4Information Provided by PolyAlloys, a division of PSM Industries |
|||
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 % |
>= 80000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys WNF-3515 Tungsten Heavy Alloy Mil. T-21014 Class 3, SAE-AMS-T-21014 Class 3, ASTM-B-777-87 Class 3Information Provided by PolyAlloys, a division of PSM Industries |
|||
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 % |
>= 80000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys WNF-7129 Tungsten Heavy Alloy Mil. T-21014 Class 1, SAE-AMS-T-21014 Class 1, AMS 7725 B, ASTM-B-777-87 Class 1Information Provided by PolyAlloys, a division of PSM Industries |
|||
Tensile Strength, Yield | 552 MPa | 80000 psi | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Tensile Strength, Yield | 552 MPa | 80000 psi | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Tensile Strength, Yield | 552 - 689 MPa @Strain 0.200 % |
80000 - 100000 psi @Strain 0.200 % |
|
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper AT(TF00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Tensile Strength, Yield | 552 - 689 MPa @Strain 0.200 % |
80000 - 100000 psi @Strain 0.200 % |
|
IBC Advanced Alloys C17510 Beryllium Copper Alloy Rounds, Temper AT(TF00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Tensile Strength, Yield | 552 MPa @Strain 0.200 % |
80100 psi @Strain 0.200 % |
|
Haynes Ultimet® alloy, aged 1000 hours at 316°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 552 - 724 MPa @Strain 0.200 %, Thickness <=25.4 mm |
80000 - 105000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Tensile Strength, Yield | 552 MPa | 80000 psi | |
Universal Wire Works E81T1-Ni2 Flux Cored Carbon Steel Tubular Electrode Alloys 81T1-Ni1 and Ni2 are designed for gas-shielded flux cored welding of low alloy steels that require good CVN toughness at subzero temperatures. These alloys are excellent for single and multip.. |
|||
Tensile Strength, Yield | 552 MPa | 80000 psi | Stress relieved |
California Fine Wire Alloy 52 Nickel Iron Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 552 MPa | 80000 psi | Stress relieved |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 552 MPa @Strain 0.200 %, Temperature -196 °C |
80100 psi @Strain 0.200 %, Temperature -321 °F |
Transverse |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 552 - 655 MPa @Strain 0.200 % |
80100 - 95000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 552 - 655 MPa @Strain 0.200 % |
80100 - 95000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899L Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 % |
>= 80100 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Alloy 255 Stainless Steel, UNS S32550 Alloy 255 is a 25% chromium duplex ferritic-austenitic stainless steel designed to provide a superior combination of high strength and excellent corrosion resistance for a wide variety of applicatio.. |
|||
Tensile Strength, Yield | 552 MPa | 80100 psi | |
ATI Allegheny Ludlum Altemp® 263 Nickel-Based alloy Characteristics: high strength up to 1500°F, oxidation resistance up to 2000°FInformation provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 552 - 655 MPa @Strain 0.200 % |
80100 - 95000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899M Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 % |
>= 80000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys WNF-5421 Tungsten Heavy Alloy Mil. T-21014 Class 2, SAE-AMS-T-21014 Class 2, ASTM-B-777-87 Class 2Information Provided by PolyAlloys, a division of PSM Industries |