Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ISO METHOD 527 |
NYCOA 2046 Copolymer Nylon 6/69 extrusion, moderate melt viscosity, high strength mono.Information provided by NYCOA, Inc. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Asia Pacific) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Asia Pacific) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Asia Pacific) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® FXC810SL PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810SL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require sparkle colour effects with lowered RFI inhibitor. Colour package may effect perform.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Strength, Yield | 56.0 MPa @Temperature 22.0 °C |
8120 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 LNP* LUBRILOY* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength, Yield | 56.0 MPa @Temperature 23.0 °C |
8120 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-3A Curing Cyanate Resin HexPly® 954-3A is a 350°F (177°C) curing cyanate resin with a 400°F (204°C) glass transition temperature. Standard cure is two hours at 350°F (177°C). Glass transition temperatures can be max.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | |
Covestro Makroblend® UT-400 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 Zytel FE3734 NC010 is an unreinforced lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ISO 527 |
Eurostar Star L POM D11 POM, Injection Molded Star L POM D11 is Silicone Oil Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
Eurostar Staramide BST42 PA6, Impact Modified, Injection Molded BST42 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
Chi Mei Polylac® PA-707 ABS High gloss, high rigid |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |