Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.14 MPa
600 psi
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
Tensile Strength, Yield 4.14 MPa
600 psi
ASTM D412
Precision Polymer Engineering S50E Silicone Rubber
Red iron oxide filled, Phenyl Silicone Rubber, 45-55 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci..
Tensile Strength, Yield 4.14 MPa
600 psi
ASTM D412
Precision Polymer Engineering S60E Silicone Rubber
Red iron oxide filled, Phenyl Silicone Rubber, 55-65 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci..
Tensile Strength, Yield 4.14 MPa
600 psi
chs 20 in/min; ASTM D638
Network Polymers Softflex® 4500
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tensile Strength, Yield 4.14 MPa
600 psi
ASTM D412
Polymax® Maxelast® P1955 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 4.14 - 57.0 MPa
600 - 8270 psi
Average value: 19.9 MPa Grade Count:13
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Strength, Yield 4.14 MPa
600 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 655 Perfluoroelastomer
Chemraz® 655 is Greene Tweed’s high-temperature off-white perfluoroelastomer. Specifically developed for wafer processes with operating temperatures up to 315°C (600°F), Chemraz 655 p..
Tensile Strength, Yield 4.14 MPa
600 psi
@50% Elongation; ASTM D1414
Greene Tweed Fluoroelastomer 742 FKM
Fluoroelastomer 742 performs well in aggressive chemicals and where ultrapure materials are not required. Recommended for conventional wet and dry system applications, Fluoroelastomer 742 has a goo..
Tensile Strength, Yield 4.14 MPa

@Strain 300 %
600 psi

@Strain 300 %
ASTM D412
Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma..
Tensile Strength, Yield 4.14 MPa
600 psi
200%, post cured- 4 hours at 177°C; ASTM D412
Multibase C6-265 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 4.14 MPa
600 psi
200%, post cured- 4 hours at 177°C; ASTM D412
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 4.14 MPa
600 psi
at 200%, post cured- 2 hours at 177°C; ASTM D412
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield >= 4.14 MPa
>= 600 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 5488 Nitrile Rubber
Low temperature service Nitrile; plasticizer freeInformation provided by Seals Eastern, Inc.
Tensile Strength, Yield 4.14 MPa
600 psi
at 100%; ASTM D412
Lubrizol Estane® ALR E80A Thermoplastic Polyurethane
Type: Estane® ALR E80A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Information Provided by The Lubrizol Corporation
Tensile Strength, Yield 4.14 MPa
600 psi
at 100%; ASTM D412
Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 75AT3 is a 75A aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and..
Tensile Strength, Yield 4.14 MPa
600 psi
100% Secant; ASTM D638
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
AFFINITY™ EG 8200G Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. It exhibits high flexibility and elasticity. It can be utilized in monolayer cast film and in ..
Tensile Strength, Yield 4.14 MPa
600 psi
cured 72 hrs @ RT
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material
QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Tensile Strength, Yield 4.14 MPa

@Strain 300 %
600 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 38-034M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDiscla..
Tensile Strength, Yield 4.14 MPa

@Strain 300 %
600 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT38-034 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDi..
Tensile Strength, Yield 4.14 MPa

@Strain 300 %
600 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3965 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti..
Tensile Strength, Yield 4.14 MPa
600 psi
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
Tensile Strength, Yield 4.14 MPa

@Strain 300 %
600 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 454 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerApplications:General PurposeCove BaseInteriorMarket:AutomotiveConsumer GoodsBuilding and ConstructionProcessing Method:Extrusion and Molding..
Tensile Strength, Yield 4.14 MPa
600 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3640 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingInformation provided by PolyOne..