Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 621 MPa | 90000 psi | |
Niagara LaSalle 1144 Cold Finished Steel Bar A high manganese, medium carbon, resulphurized steel with free machining qualities and higher mechanical properties than the lower carbon steels. This grade machines at 83% of 1212 with excellent as.. |
|||
Tensile Strength, Yield | 621 MPa | 90000 psi | |
Pacific Sintered Materials FCC-214-S(HT) High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Yield | 621 MPa | 90000 psi | |
Pacific Sintered Materials FX-233-T Infiltrated Alloy Steel Excellent combination of strength and shock resistance. Good for use in cams, pawls, sprockets and wear plates. Moderate tolerance control.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 621 MPa | 90000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated Alloy Steel FX-233-T Powdered Metal Excellent combination of strength and shock resistance, Good for use in cams, pawls, sprockets and wear plates, Moderate tolerance controlInformation Provided by Pacific Sintered Metals, a division .. |
|||
Tensile Strength, Yield | 621 MPa @Temperature 23.9 °C |
90000 psi @Temperature 75.0 °F |
0° Direction, Dry, Autoclave; ASTM D638 |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 3k 5HS Carbon Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Tensile Strength, Yield | 621 MPa @Temperature 21.1 °C |
90000 psi @Temperature 70.0 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Tensile Strength, Yield | >= 621 MPa | >= 90000 psi | |
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Yield | >= 621 MPa @Strain 0.200 % |
>= 90000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 CX90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90000 psi @Strain 0.200 % |
|
Schmolz + Bickenbach MoldMAX® SC Copper Alloy Description: Brush Wellman’s MoldMAX® SC is a high conductivity copper mold alloy with good strength. MoldMAX® SC is used as blow mold cavities, injection mold cores and cavities and hot .. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90000 psi @Strain 0.200 % |
Heat Treated |
Universal Wire Works Inconel 69 (AMS 5778) Filler Metal Inconel Filler Metal 69 is used for gas tungsten arc and gas metal arc welding of Inconel Alloy 722 and Inconel x-750. Typical applications for filler metal 69 include gas turbine and aircraft parts.. |
|||
Tensile Strength, Yield | 621 - 731 MPa | 90000 - 106000 psi | 0.2% offset |
Eagle Brass 770 Nickel Silver 18%, Hard 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | Forgings |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | |
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | >= 621 MPa @Strain 0.200 % |
>= 90000 psi @Strain 0.200 % |
|
Dura-Bar 120-90-02 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | |
CMW® THERMKON® 70M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | 621 - 689 MPa @Strain 0.200 % |
90100 - 99900 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 621 - 689 MPa @Strain 0.200 % |
90100 - 99900 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899L Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 621 - 689 MPa @Strain 0.200 % |
90100 - 99900 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899M Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® H-46 Specialty Steel, Heat Treatment: 1149°C (2100°F) Anneal Data provided by Allvac.Applications: Structural components for land-based turbine engines. Rings and structurals in jet engines. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal Data provided by Allvac.Applications: Jet engine components, exhaust manifold heat exchangers, chemical process equipment, semiconductor systems. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 410/403 Specialty Steel, Heat Treatment: 927°C (1700°F) Anneal Data provided by Allvac.Applications: Compressor blades, turbine parts. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90000 psi @Strain 0.200 % |
|
Carlson 303 Austenitic Stainless Steel Carlson 303 is an austenitic free-machining stainless steel. The standard 18-8 stainless steels are more difficult to turn, mill and drill which restricts their use when considerable machining is r.. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | Age Hardened per AMS 5872D, 21°C |
ATI Allegheny Ludlum Altemp® 263 Nickel-Based alloy Characteristics: high strength up to 1500°F, oxidation resistance up to 2000°FInformation provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | >= 621 MPa @Strain 0.200 % |
>= 90100 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 1 Cold Worked Level 1 Cold Worked applies to tensile properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |
|||
Tensile Strength, Yield | >= 621 MPa @Strain 0.200 % |
>= 90000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 AT90 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | |
HP Alloys HPA COBALT Alloy 6B, Wear Resistant, (Co-Cr-W) (UNS R30016) Cobalt 6B is a cobalt based chromium, tungsten alloy for wear environments where seizing, galling and abrasion are present. 6B is resistant to seizing and galling and with its low coefficient of fri.. |
|||
Tensile Strength, Yield | >= 621 MPa @Strain 0.200 % |
>= 90100 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 1 Cold Worked Cold Worked applies to tensile values and are for 0.25" to 4" diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resistanc.. |