Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUCON CP6052 PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, Low Surface Resistivity, Improved Impact StrengthApplication: Laser diode Tray, ATM parts, Telecommunication Station Housi.. |
|||
Tensile Strength, Yield | 63.7 MPa @Thickness 3.20 mm |
9250 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUMID HI1102B(W) PA66, High Impact Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Tensile Strength, Yield | 63.7 MPa | 9240 psi | ASTM D638 |
Kostat KAH1 Heat Seal Activated Cover tapes KOSTATs KAH1 series of Heat Seal Activated Cover Tape is manufactured using Antistatic Polyethylene Terephthalate film and other proprietary adhesive materials. The component for its anti-static pr.. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® FD-1122 PC, FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HR-8070 MPPE, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NF-3017 PC/ABS, Unreinforced FR Flame-retardant scratch resistant material that can be used in notebook B partInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® SC-1100R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® UF-1013 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TH-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® FD-1122 PC, FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HR-8070 MPPE, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NF-3017 PC/ABS, Unreinforced FR Flame-retardant scratch resistant material that can be used in notebook B partInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® SC-1100R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TH-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® UF-1013 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 63.7 MPa | 9250 psi | ASTM D638 |
Cheng Yu Plastic PP238G3 Polypropylene, 30% Glass Fiber |
|||
Tensile Strength, Yield | 63.7 MPa | 9240 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers SAN 280 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |