Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 750 - 1050 MPa | 109000 - 152000 psi | Swaged after Sintering |
MarkeTech 97-2-1 Tungsten Alloy, AMS-T-21014 Class 4 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Yield | 750 - 940 MPa | 109000 - 136000 psi | |
Materion Beryllium Copper Alloy 190 Strip; HM (TM04) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 68%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 750 MPa @Strain 0.200 %, Temperature 760 °C |
109000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Tensile Strength, Yield | 750 MPa @Strain 0.200 % |
109000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals NIMONIC® Alloy PK33 A nickel-chromium-cobalt alloy that is precipitation hardenable and also contains a relatively high (7%) level of molybdenum for solid-solution strengthening. It has an exceptional combination of h.. |
|||
Tensile Strength, Yield | 750 MPa @Temperature 135 °C |
109000 psi @Temperature 275 °F |
90º, Wet; EN2561 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon Information provided by HexCel |
|||
Tensile Strength, Yield | 750 MPa @Strain 0.200 % |
109000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 80 Thickness >80-100 mm Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the h.. |
|||
Tensile Strength, Yield | 750 MPa @Strain 0.200 % |
109000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 80 Thickness 16-80 mm Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the h.. |
|||
Tensile Strength, Yield | 750 MPa @Strain 0.200 % |
109000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 80 Thickness 5 - Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the h.. |
|||
Tensile Strength, Yield | 750 MPa @Strain 0.200 % |
109000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 80PV Thickness >80-100 mm A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Tensile Strength, Yield | 750 MPa @Strain 0.200 % |
109000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 80PV Thickness 6- A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Tensile Strength, Yield | 750 - 950 MPa | 109000 - 138000 psi | |
ArcelorMittal Complex Phase Steel 1000 SF Very high strength steel, Cold Rolled Steel Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product range. These steels are cold formed to make lightweight structural elements. A num.. |
|||
Tensile Strength, Yield | 750 MPa @Strain 0.200 % |
109000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 80PV Thickness 16-80 mm A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |