Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1700 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1701 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1705 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1710 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1750 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1760 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1800 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1801 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1810 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1850W Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1751 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | >= 520 MPa | >= 75400 psi | |
H.C. Starck HPM 1850 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
Tensile Strength, Yield | 520 MPa @Strain 0.200 %, Temperature 650 °C |
75400 psi @Strain 0.200 %, Temperature 1200 °F |
Precipitation Hardened prior to test |
Special Metals NIMONIC® Alloy 81 A precipitation-hardenable nickel-chromium alloy with enhanced resistance to high-temperature corrosion. The excellent hot-corrosion resistance of the alloy results from its high chromium content o.. |
|||
Tensile Strength, Yield | 520 MPa | 75400 psi | |
Elgiloy® Co-Cr-Ni Alloy, Strip General Elgiloy® information: High strength, ductility, fatigue life, and good mechanical properties. Corrosion resistant in numerous environments. Available in strip (currently 0.0015" to 0.075".. |
|||
Tensile Strength, Yield | 520 MPa @Strain 0.200 % |
75400 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 29-4C® Stainless Steel, UNS S44735 AL 29-4C alloy is a superferritic stainless steel designed by Allegheny Ludlum for extreme resistance to chloride ion pitting, crevice corrosion and stress corrosion cracking, as well as general cor.. |