Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 77.0 MPa | 11200 psi | ISO 527-2 |
PolyOne Trilliant™ HC THC-02 1200 IL Natural Polyamide 66 (Nylon 66) The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ah.. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT4143T PC Copolymer (Asia Pacific) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | 10%/min. ASTM D638 |
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan.. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp OF003A PPS LNP* Thermocomp* OF003A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific) Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp OF003A PPS (Asia Pacific) LNP* Thermocomp* OF003A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix HexPly® M42 is a high performance, self extinguishing, self adhesive, tough epoxy matrix for use in primary aerospace sandwich structures. It exhibits very high impact resistance and damage toleran.. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | 50 mm/min; ISO 527 |
Chi Mei Kibisan® PN-127 SAN Heat Resistant |
|||
Tensile Strength, Yield | 77.0 MPa @Temperature 23.0 °C |
11200 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 1061 Polyimide, 15% Graphite, 10% PTFE Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Conditioned (2.5% Moisture) Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | ISO 527 |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, Conditioned Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Tensile Strength, Yield | 77.0 MPa | 11200 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL PX2907 PPE+PS (Asia Pacific) PPE+HIPS GF10% FR V-1 |