Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.30 MPa | 1200 psi | 20 in/min, injection molded, type 1 specimen; ASTM D638 |
Phillips Sumika Marlex® CHP-015 Thermoplastic Polyolefin
(discontinued **) Applications: Driver-side air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 201.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | 500 mm/min; ASTM D638 |
Eastman D4056-P Polyethylene
(discontinued **) Polyethylene D4056-P is a natural low density material with an 80 melt index.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no lon.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | |
Kraton® D1102 + LDPE blend (20/80) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Tensile Strength, Yield | 8.30 MPa @Strain 100 % |
1200 psi @Strain 100 % |
ASTM D638 |
Toyobo E3090A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information .. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | ASTM D638 |
Chevron Phillips Marlex® 1007 Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 25200Characteristics: Excellent Flexibility, Good Flow, Good Warping Resistance, Moderate Mold Release, Good ESCRApplications:Houseware.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Softflex® SF 5560 Overmold for Nylon Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | |
Dow AFFINITY™ SM 1350 Polyolefin Plastomer AFFINITY® SM 1350 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in durable injection molded housewares and compression molded closure liners or gaskets. It exhibit.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8445 Polyolefin Elastomer Description: Engage® 8445 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | Molded property |
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl.. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Softflex® 1701-1402 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | Molded property |
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Tensile Strength, Yield | 8.30 MPa | 1200 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8540 Polyolefin Elastomer Description: Engage® 8540 polyolefin elastomer is an ethyleneoctene copolymer that is well suited to foamed applications and offers excellent performance for profile extrusion of tubing and hoses. .. |
|||
Tensile Strength, Yield | 8.30 - 21.0 MPa | 1200 - 3050 psi | Average value: 11.5 MPa Grade Count:59 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |