Mechanical Properties Metric English Comments
Tensile Strength, Yield 820 MPa

@Strain 0.200 %,
Temperature 650 °C
119000 psi

@Strain 0.200 %,
Temperature 1200 °F
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 820 MPa

@Strain 0.200 %
119000 psi

@Strain 0.200 %
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 820 MPa

@Temperature 24.0 °C
119000 psi

@Temperature 75.2 °F
Dry
Hexcel® HexPly® F522 Epoxy Resin, F3C584 Carbon Fabric
Hexcel designation: F3C584-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel
Tensile Strength, Yield 820 MPa

@Temperature 23.0 °C
119000 psi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, AS4-C
Fiber Designation: C193PW, Plain weaveInformation provided by HexCel