Tensile Strength, Yield 595 MPa

@Strain 0.200 %
86300 psi

@Strain 0.200 %
Haynes 214® alloy, 0% cold reduction
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 595 MPa

@Strain 0.200 %
86300 psi

@Strain 0.200 %
Haynes 214® alloy, 40% cold reduction, 1095°C (2000°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 595 MPa

@Strain 0.200 %,
Temperature 425 °C
86300 psi

@Strain 0.200 %,
Temperature 797 °F
Haynes 242® alloy, bar and rings, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 595 MPa

@Strain 0.200 %,
Temperature 760 °C
86300 psi

@Strain 0.200 %,
Temperature 1400 °F
Haynes 25 alloy, cold worked sheet, 15 % cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 595 MPa

@Strain 0.200 %
86300 psi

@Strain 0.200 %
Haynes 230® alloy, 50% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..