Polymer Property : Tensile Strength, Yield = 9.70 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.70 MPa
1410 psi
500 mm/min; ASTM D638
Eastman E6838-889P Polyethylene  (discontinued **)
Polyethylene E6838-889P is a formulation suggested for extrusion coating applications and has been used successfully in compounding. This product may be used for holding food during cooking.Applicat..
Tensile Strength, Yield 9.70 MPa
1410 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman 808E Polyethylene  (discontinued **)
Low density polyethylene 808E is a general-purpose formulation used general-purpose extrusion. Under regulations administered by the US FDA, 808E may lawfully be used as articles or components of a..
Tensile Strength, Yield 9.70 MPa
1410 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman E6838-850P Polyethylene  (discontinued **)
E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seal..
Tensile Strength, Yield 9.70 MPa
1410 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman E6838-862A Polyethylene  (discontinued **)
E6838-862A is a low density formulation suggested for injection molding applications, such as closuresInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemic..
Tensile Strength, Yield 9.70 MPa
1410 psi
Molded property
Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2244A Polyethylene resin is a cast film polymer having superior optics in packaging applications. This material complies with U.S. FDA Regulation 21 CFR 177.1520 c 3.2 (a) food packaging ap..
Tensile Strength, Yield 9.70 MPa

@Strain 50.0 %
1410 psi

@Strain 50.0 %
50 mm/min
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista..