Polymer Property : Tensile Strength, Yield = 900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.21 MPa
900 psi
TM R050-36
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11..
Tensile Strength, Yield 6.21 MPa
900 psi
TM R050-36
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D638
Multibase Multi-Flex® D 4210 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, GoodStiffness, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation p..
Tensile Strength, Yield 6.21 MPa
900 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 7025 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tensile Strength, Yield 6.21 MPa
900 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7130 Fluorocarbon-Elastomer
FKM specially for oil & gas service.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 6.21 MPa
900 psi
Tensile strength decreases by 10% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Saint-Gobain COHRlastic® 9040 Wide Series General Purpose Silicone Solid Rubber
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome..
Tensile Strength, Yield 6.21 MPa
900 psi
100%; ASTM D412
Teknor Apex APEX® 3211-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Tensile Strength, Yield 6.21 MPa
900 psi
100%; ASTM D412
Teknor Apex APEX® 3300-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex MONPRENE® MP 2830M Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex MONPRENE® MP 2835E Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
Tensile strength decreases by 10% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Saint-Gobain COHRlastic® 9050 Wide Series General Purpose Silicone Solid Rubber
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome..
Tensile Strength, Yield 6.21 MPa
900 psi
100%; ASTM D412
Teknor Apex APEX® 3200-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex TEKBOND® 6000-35 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex TEKBOND® 6000-75 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex TEKRON® 4000-40 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 6.21 MPa
900 psi
at 200%; ASTM D412
Lubrizol Estane® ALR E80A Thermoplastic Polyurethane
Type: Estane® ALR E80A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Information Provided by The Lubrizol Corporation
Tensile Strength, Yield 6.21 MPa
900 psi
at 300%; ASTM D412
Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 75AT3 is a 75A aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and..
Tensile Strength, Yield 6.21 MPa
900 psi
at 100%; ASTM D412
Lubrizol Estane® MVT 90AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 90AF3 TPU is a 90A aromatic polyether-based thermoplastic polyurethane.Features: High moisture vapor transmission, good physical properties and elasticity, free of organo-tin comp..
Tensile Strength, Yield 6.21 MPa

@Temperature 21.1 °C
900 psi

@Temperature 70.0 °F
Flatwise Tensile; 15 Cycles, Thermal Cycling
Hexcel® Redux® HP655 Toughened BMI film Adhesive
Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655..
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D638
Clariant Renol PUR1100SS15 Polyurethane Elastomer, Stainless Fiber, EMI/RFI/ESD
Data provided by Clariant Masterbatches
Tensile Strength, Yield 6.21 MPa
900 psi
ASTM D412
Teknor Apex Monprene® MP-2835E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength, Yield 6.21 MPa
900 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® IT 36-021 NATURAL Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Specialty Thermoplastic ElastomerApplications: FDA (Food Contact)Processing Method: Injection MoldingInformation provided by PolyOne Corporation
Tensile Strength, Yield 6.21 MPa
900 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3945 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti..
Tensile Strength, Yield 6.21 MPa
900 psi
TM R050-36
Resinlab® EP1026R Rubber Modified Epoxy Adhesive
Resinlab™ EP1026R is a two part unfilled rubber modified epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free ..