Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.80 GPa | 261 ksi | ISO 527-1,2 |
Qualchem Danamid FEL0 Polyamide 6 Flame retardant, with halogens (V-0)Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 1.80 GPa @Temperature 100 °C |
261 ksi @Temperature 212 °F |
ISO 527 |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |
|||
Tensile Modulus | 1.80 - 2.50 GPa @Thickness 2.00 mm, Temperature 23.0 °C |
261 - 363 ksi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | 1 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS M406 Lustran® ABS M406 has very high impact strength and increased chemical and dynamic resistance. It is used for the production of molded plastic articles. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ISO 527 |
Styrolution PS 486N HIPS Styrolution PS 486N is a normal flowing, high impact grade that is especially suitable for blends with a high proportion of general purpose polystyrene (preferably Styrolution PS 165N of Styrolution.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ISO 527-1/-2 |
Unitika A1025NO PA6, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ASTM-D790 |
Polyram RamLloy PBB702 PC/ABS alloy, UV Stabilized UV stabilized PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ASTM D638 |
Goodfellow TPX® DX350 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ISO 527-2 |
Total PPC 1645 Polypropylene, Heterophasic Copolymer, Pipes Polypropylene PPC 1645 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It offers a very high stiffness .. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ISO 527 |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4188 black 9992 PA612 Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4188 nat PA612 Product description: Grilamid XE 4188 natural is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 natural are: High viscosi.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | DIN 53 457 |
Hippe PA 11 Nylon 11 Water armatures, bearing under water, seals, housings, fans, insulated parts, parts for textile machines and household units. Toother wheels, sliding components and guides. Very low water absorpti.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide P1000EI3 PA6, Impact Modified, Injection Molded Staramide P1000EI3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020)Information provided by Eurostar. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ASTM D638 |
Aclo Accucomp Polycarbonate POL051L Medium Viscosity |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ASTM D638 |
Aclo Accucomp Polycarbonate POL052L High Viscosity |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334M10CL Mica Reinforced Coupled |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | |
BASF Polystyrol® 486 M Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H). Suitable for dairy packaging.Data was co.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8350 HS BK-102 PA6 (Dry) Ultramid 8350 HS BK-102 is a type 6, black pigmented, impact modified graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness
combined with a.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8350 HS PA6 (Dry) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436T20L1 Talc Reinforced |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | ASTM D638 |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Tensile Modulus | 1.80 GPa | 261 ksi | 50% RH; ISO 527 |
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion
(discontinued **) AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil.. |