Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1.862 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.862 GPa
270.1 ksi
ASTM D638
Resirene Resirene® 6420 Super High Impact Polystyrene
Features:Super High ImpactEasy ProcessingLow ModulusFlexibilityFDA Rating: 21 CFR 177.1640Applications:ExtrusionDeep ThermoformingGPPS/HIPS BlendsPoint of Purchase DisplaysInformation provided by US..
Tensile Modulus 1.862 GPa
270.1 ksi
ASTM D638
Resirene Resirene® READ 9500 Ignition Resistant Impact Polystyrene
Features:High FlowIgnition ResistantNo Pre-drying RequiredHigh ImpactColors AvailableApplications:Injection MoldingDark ColorsTV CabinetsElectronic EquipmentInformation provided by US distributor Ca..
Tensile Modulus 1.862 GPa
270.1 ksi
ASTM D638
Resirene Resirene® 8450 High Impact Polystyrene (Chemical Resistant)
Features:Low FlowChemical ResistantMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:Extrusion/ThermoformingRegistration LinersExtruded SheetInformation provided by US distributor Calsak Co..
Copyright © lookpolymers.com All Rights Reserved