Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.3 GPa | 1490 ksi | ISO 527-1/2 |
Radici Radilon® CARV300 L (dry) Copolyamide 66/6 Glass-fiber reinforcedInformation provided by Radici group. |
|||
Tensile Modulus | 10.3 GPa | 1500 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)
(discontinued **) Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 10.3 GPa | 1500 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ CTX 1125 PC/ABS Blend, Carbon Fiber Reinforced
(discontinued **) Description/Features:Electrically ConductiveNickel Coated Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 10.3 GPa | 1500 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 10.3 GPa | 1500 ksi | |
MTI ThermoStran® PP-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | ASTM D638 |
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | ASTM D638 |
Plenco 1501 Polyester, Pellet, Injection Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Tensile Modulus | 10.3 GPa | 1500 ksi | ASTM D638 |
Ecomass® 1850ZG92 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T.. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | |
Radici Radilon® A RV300 990 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |