Polymer Property : Tensile Modulus = 10.56 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 10.56 GPa
1532 ksi
ASTM D638
Plenco 50030 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..
Tensile Modulus 10.56 GPa
1532 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear (Asia Pacific)
LNP* STAT-KON* OEP32 is a compound based on PPS - Linear resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive.
Tensile Modulus 10.56 GPa
1532 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear
LNP STAT-KON* OEP32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.