Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.92 GPa | 1729 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 11.92 GPa | 1729 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 LNP* KONDUIT* RTF2B is a compound based on Nylon 66 resin containing 10% Glass Fiber, 55% Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 11.92 GPa | 1729 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 11.92 GPa | 1729 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP QFL17RS PA 6/10 LNP LUBRICOMP* QFL17RS is a compound based on Nylon 6/10 resin containing 35% Glass Fiber, 5% PTFE. Added features of this material include: Easy Release, Heat Stabilized, Wear Resistant. |