Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.72 GPa | 1120 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ AS-13CF/000 Black Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ISO 527-1,2 |
Qualchem Danamid FGFLX2-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 7.72 GPa | 1120 ksi | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | |
LATI Latigray 82-02 CX/80 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Tensile Modulus | 7.71 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 7.71 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 7.71 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Tensile Modulus | 7.74 GPa | 1120 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 (Asia Pacific) LNP* Thermocomp* RFB53XXZ is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. |
|||
Tensile Modulus | 7.72 GPa | 1120 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 7.72 GPa | 1120 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific) LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL EM7430 PPE+PS 30% glass reinforced, high flow PPO. Automotive. Energy management material. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | ASTM D638 |
Plenco 7500 Phenolic, Granular, Transfer Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | ISO 527 |
Polyram Polytron P30N11 Polypropylene, 30% Long Fiber Glass A chemically coupled 30% long fiber glass reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 7.72 GPa | 1120 ksi | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Tensile Modulus | 7.72 - 7.93 GPa | 1120 - 1150 ksi | 20% Glass Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | ASTM-D790 |
Polyram Polytron P30N01 Homopolymer Polypropylene, Chemically Coupled 30% Long Fiber A CHEMICALLY COUPLED 30% LONG FIBER GLASS REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 7.70 GPa | 1120 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-25/4 PA666-GF25 Information provided by EMS Grivory |
|||
Tensile Modulus | 7.72 GPa @Temperature -20.0 °C |
1120 ksi @Temperature -4.00 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Modulus | 7.69 GPa | 1120 ksi | 1 mm/min |
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Tensile Modulus | 7.70 GPa @Temperature -40.0 °C |
1120 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Conditioned) Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi.. |
|||
Tensile Modulus | 7.75 GPa @Temperature -35.0 °C |
1120 ksi @Temperature -31.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Modulus | 7.75 GPa | 1120 ksi | ASTM-D790 |
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |