Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 90.0 - 120 GPa | 13100 - 17400 ksi | |
Goodfellow Phosphor Bronze Good Machinability. Uses include springs, clips, gauzes and architectural applicationsInformation provided by Goodfellow. |
|||
Tensile Modulus | 110 - 120 GPa | 16000 - 17400 ksi | Longitudinal |
Goodfellow Carbon/Epoxy Composite Tube Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |