Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.89 GPa | 1290 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | |
LATI Latigray 82-03 CW/96 F3 PA 12, Metallic Reinforced Radiopaque compound based on Polyamide 12 (PA12). Metallic filler. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America;.. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240A PP SABIC® PPcompound G3240A is a general purpose, 40% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 139448304. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240U PP SABIC® PPcompound G3240U is a general purpose, 40% glass filled, chemically coupled, heat stabilized and UV stabilized homopolymer polypropylene compound. The IMDS ID is 209768078. |
|||
Tensile Modulus | 8.89 GPa | 1290 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 8.89 GPa | 1290 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su.. |
|||
Tensile Modulus | 8.89 GPa | 1290 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 8.89 GPa | 1290 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare |
|||
Tensile Modulus | 8.89 GPa | 1290 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East) High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 8.89 GPa | 1290 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Tensile Modulus | 8.92 GPa | 1290 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 LNP* STAT-KON* RFD03 is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KFZ24XXP Acetal Copoly LNP* THERMOCOMP* KFZ24XXP is a compound based on Acetal Copolymer resin containing 20% Glass Fiber, 10% Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled, Inter.. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WX93111 PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* WX93111 is a compound based on Polybutylene Terephalate resin containing Flame retardant , Glass Fiber, Proprietary filler. Added features include : Improved CTI. |
|||
Tensile Modulus | 8.91 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Tensile Modulus | 8.92 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend High flow Ultem for thin wall application |
|||
Tensile Modulus | 8.91 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF CF007IXP PS LNP* Thermotuf* CF007IXP is a compound based on Polystyrene containing glass fiber. Characteristics of this grade are: High Impact. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | ISO 527-1/-2 |
DSM Stanyl® TW271F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, PTFE Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | ISO 527-1/-2 |
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 ZYTEL FR95G25V0NH NC010 is 25% glass fiber reinforced flame retardant polyamide halogen and red phosphorous free with high flow and excellent long t.. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF5 POM 26% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Tensile Modulus | 8.91 GPa | 1290 ksi | ISO 527 |
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Conditioned) Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu.. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | ISO 527 |
Eurotec® Tecomid® NB40 KK40 NL PA6, 40% glass fiber/mineral reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 8.89 GPa | 1290 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP IF007 PA6.12 LNP THERMOCOMP* IF007 is a compound based on Nylon 6/12 resin containing 35% Glass Fiber. |
|||
Tensile Modulus | 8.92 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
Tensile Modulus | 8.92 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Tensile Modulus | 8.90 GPa | 1290 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36 PSU (Europe-Africa-Middle East) LNP* Lubricomp* GFL36 is a compound based on Polysulfone resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |