Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.45 GPa | 1370 ksi | ASTM D638 |
NYCOA ASN 27 300 KNF 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6 Resin NYCOA ASN 27 300 KNF is a 30% glass fiber reinforced, heat stabilized Nylon 6 resin used for injection molding. This grade features excellent strength and stiffness, dimensional stability, and a gre.. |
|||
Tensile Modulus | 9.45 GPa | 1370 ksi | |
Haveg 41NA Phenolic; Silicate Filled A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers. |
|||
Tensile Modulus | 9.44 GPa | 1370 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Tensile Modulus | 9.45 GPa | 1370 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP JF006 PES LNP* THERMOCOMP* JF006 is a compound based on Polyethersulfone resin containing 30% Glass Fiber. |
|||
Tensile Modulus | 9.44 GPa | 1370 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Tensile Modulus | 9.44 GPa | 1370 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Tensile Modulus | 9.42 GPa | 1370 ksi | ASTM D638 |
Plenco 50335 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |
|||
Tensile Modulus | 9.47 GPa | 1370 ksi | ASTM D638 |
Plenco 50335 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |