Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.5 GPa | 2100 ksi | |
Plastcom SLOVAMID 6 GF 50 TS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-2 |
PolyOne OnForce™ LFT NY-50LGF/001 HS Natural Polyamide 6 (Nylon 6) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Therma-Tech™ NNC-5000 TC Polyamide 66 (Nylon 66) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 50 Polyamide 6, 50% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | |
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Modulus | 14.5 GPa @Temperature 23.0 °C |
2100 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® LC-30GF/000 LCP (Liquid Crystal Polymer), 30% Glass Reinforced, Hi-Temp
(discontinued **)< Information provided by PolyOne™ Corporation |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | tangent; ASTM D638 |
Premix Premi-Glas® 8102-20 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8102-20 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Therma-Tech™ NJC-7500 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | cond; ISO 527-1/-2 |
DSM Stanyl® TW271B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 45 HWCP 45% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | cond; ISO 527-1/-2 |
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1 |
Barlog Plastics KEBAFLOW MF130 LCP, 30% glass fiber reinforced LCP-GF30Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1 |
Barlog Plastics KEBATRON C2040G5 PPS, cross-linked, 40% GF, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1 |
Barlog Plastics KEBATRON L1040G3 PPS, linear, 40% glass fiber reinforced PPS-GF40Information provided by BARLOG plastics GmbH. |