Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 152 GPa | 22000 ksi | |
PSM Industries Pacific Sintered Metals 4600 F-253-T(HT) Powdered Metal High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-140HTInformation Provided by Pacific Sintered Metals, a division of PSM .. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | 0°; ASTM D3039 |
Zyvex Performance Materials Arovex™ 250 Carbon Nanotube Strengthened Prepreg Arovex® 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (121°.. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | Typical epoxy composite property |
Hexcel® HexTow™ AS7 Carbon Fiber HexTow™ AS7 carbon fiber is a continuous, high strength, high strain, PAN based fiber available, in a 12,000 (12K) filament count tow. This fiber has been surface treated and can be sized to improv.. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | |
Eagle Brass 715 Copper Nickel 30%, 1/2 Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | |
Eagle Brass 715 Copper Nickel 30%, 1/4 Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | |
Eagle Brass 715 Copper Nickel 30%, Annealed 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | |
Eagle Brass 715 Copper Nickel 30%, Extra Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | |
Eagle Brass 715 Copper Nickel 30%, Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | |
Eagle Brass 715 Copper Nickel 30%, Spring 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-10 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-10 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-10 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-12 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-11 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-11 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-12 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-20 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-30 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-40 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-62 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tensile Modulus | 152 GPa | 22000 ksi | Typical epoxy composite property |
Hexcel® HexTow™ AS4D Carbon Fiber HexTow™ AS4D carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized to improve .. |
|||
Tensile Modulus | 152 GPa | 22000 ksi | filament |
3M Nextel™ AF-14 Industrial Woven Fabric 312 Information provided by 3M |