Mechanical Properties Metric English Comments
Tensile Modulus 12.8 GPa
1860 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral filled PA6 compound
Tensile Modulus 12.8 GPa
1860 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Stat-Tech™ NN-20CF/000 Black HS Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Tensile Modulus 12.8 GPa
1860 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Stat-Tech™ NN-20CF/000 Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Tensile Modulus 12.8 GPa
1860 ksi
ASTM D638
LNP Lubricomp® PDX-U-95672 BK8-115 Polyphthalamide, Proprietary Filler  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Tensile Modulus 12.8 GPa
1860 ksi
ISO 527
Nilit FRIANYL A63 HS-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 12.8 GPa
1860 ksi
LATI Laticonther 82 CP1/800 PA12
High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Tensile Modulus 12.8 GPa
1860 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear
LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant.
Tensile Modulus 12.8 GPa
1860 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear
LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant.
Tensile Modulus 12.8 GPa
1860 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
Tensile Modulus 12.8 GPa
1860 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ507 PBT+PC
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Tensile Modulus 12.8 GPa
1860 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Tensile Modulus 12.8 GPa
1860 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Tensile Modulus 12.8 GPa
1860 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR
LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 12.8 GPa
1860 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12
LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber.
Tensile Modulus 12.8 GPa
1860 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East)
Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 12.8 GPa
1860 ksi
1 mm/min; ISO 527-1
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber
SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers
Tensile Modulus 12.8 GPa
1860 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific)
Glass filled Nylon 12
Tensile Modulus 12.8 GPa
1860 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50
Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p..
Tensile Modulus 12.8 GPa
1860 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Tensile Modulus 12.8 GPa
1860 ksi
Plastcom SLOVALEN PH 49 GF 60 PP reinforced with 60% glass fibre
Features: Modified homopolymer PP for injection moulding, chemically reinforced with 60% glass fibre, contains the modifier of mechanical properties.Very good strength and tensile modulus. Delivered..