Polymer Property : Tensile Modulus = 19700 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 136 GPa
19700 ksi
Longitudinal
Goodfellow Carbon/Vinyl Ester Rod
Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow.
Tensile Modulus 136 GPa
19700 ksi
Longitudinal
Goodfellow Carbon/Vinyl Ester Tube
Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow.
Tensile Modulus 136 GPa
19700 ksi
Typical epoxy composite property
Hexcel® HexTow™ AS2C Carbon Fiber
HexTow™ AS2C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated..