Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® X TR2-10TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Europe-Africa-Middle East) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM D638 |
Ineos Nova Zylar® 220 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarity Good elongation Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class VI plasticsApplications:D.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Spartech Acrylloy 7 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Spartech Tuf-Glas Impact Modified Acrylic Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon WX98547 PBT LNP* Stat-kon* WX98547 is a compound based on Polybutylene Terephalate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SAB.. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Star Plastics ABS3030 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Star Plastics ABS9020 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM Test |
Styrolution Terblend® N NM-12 ABS/PA6 (Dry) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM Data |
Styron Magnum™ 9095 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP LNP* THERMOCOMP* MF001AS is a compound based on Polypropylene resin containing 5% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Total PSI 825 Polystyrene Polystyrene 825 is a high impact polystyrene for injection molding. They polymers ability to be molded on fast cycles with minimal stresses results in outstanding impact retention.Applications such .. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D638 |
Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 2.28 GPa | 330 ksi | ASTM D-638 |
Axiall UV-6685 Rigid PVC, Molding Georgia Gulf UV 6685 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of parts requiring resistance to outdoor UV degradation.Info.. |