Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.45 GPa | 355 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PH 91 T 20 Polypropylene reinforced with mineral filler Modified homopolymer PP for injection molding with the content of 20 % mineral filler. General application in all industry branches. Delivered in natural mode and in the full RAL color scale.Informa.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ H PC DP113/X5 Polycarbonate Polycarbonate-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG94 ABS Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/-2 |
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data) Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EX7631T PC EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP D1000 PC (Europe-Africa-Middle East) LNP* COLORCOMP* D1000 is a compound based on Polycarbonate resin containing Unfilled Custom Color |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC (Asia Pacific) LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | |
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min |
Polimeri Europa EDISTIR PD RK4122H High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,078-06-04-23 UL94 V-2, halogen and antimony free, medium impact polystyrene. This grade features enhanced thermal stabi.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPS7 PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPS7 PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | |
Ineos Styrenics Polystyrene 147F (NAFTA) An easy flow, general purpose polystyrene. Has moderate heat resistance and strength for general molding and extrusion applications.Information provided by BASF.Ineos Styrenics purchased this produ.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1040 PP SABIC® PPcompound 55T1040 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact and high rigidity, and is suitable for injec.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DSL229 PC LNP* STAT-KON* DSL229 is a compound based on Polycarbonate resin containing 10% PTFE, 10% Stainless Steel. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1mm/min; ISO 527 |
Teijin Panlite® AD-5503 Optical Use Polycarbonate Resin High fluidity grade for optical media that provides low optical distortion moldings. Impurities in pellets are severely controlled, and resulting high quality is obtaining good reputation.Applicatio.. |
|||
Tensile Modulus | 2.45 GPa | 356 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/-2 |
Covestro Bayblend® W85 XF* Polycarbonate + ASA Developmental product(PC+ASA) blendinjection molding grade with improved weather resistanceoptimized heat ageing stabilityhigh heat resistanceVicat/B 120 = 132 °CPreprocessingMax. Water content |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | |
Dow SiLK™ I 130 Semiconductor Dielectric Resin SiLK™ I 130 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 130 is compatible with.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | |
Dow SiLK™ I 620 Semiconductor Dielectric Resin SiLK™ I 620 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 620 is compatible with.. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | |
BASF Polystyrol® 445 E WU Impact Grade Polystyrene (Europe) Easy flowing, heat-resistant, medium-impact, flame-retardant grade. Application example: electrical distribution boxes.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/2 |
BLUESTAR BS090 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | ISO 527-1/-2 |
BASF Ultraform® N2320 0035 POM Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF |
|||
Tensile Modulus | 2.45 GPa | 355 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |