Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.48 GPa | 360 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87850 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products
(discontinued **) ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and .. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
(Unverified Data**) Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
(Unverified Data**) Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
(Unverified Data**) Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
(Unverified Data**) Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC (Asia Pacific) LNP* STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU) Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU) Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific) LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D638 |
Styrolution PS-148G Polystyrene Description: Polystyrene 148G is a high heat, easy flow general purpose polystyrene with excellent moldability, clarity and fast set-up time. It can be utilized as a coextruded gloss cap over high i.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP NX10302 PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM Data |
Styron CALIBRE™ 200 4 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM Data |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific) Low odor grade for IC tray application |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Europe-Africa-Middle East) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM Data |
Styron Magnum™ 341 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D-638 |
Axiall 8258 Rigid PVC, Extrusion Georgia Gulf 8258 is a special purpose rigid PVC for film and food grade sheet compound. It has been used where packages are manufactured to FDA guidelines.Information provided by Georgia GulfGeorg.. |
|||
Tensile Modulus | 2.48 GPa | 360 ksi | ASTM D-638 |
Axiall 9129J Rigid PVC, Extrusion Georgia Gulf 9129J is designed for use in extruded price tag holders. The compound contains an ultraviolet light stabilizer which retards color change.Information provided by Georgia GulfGeorgia Gu.. |