Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY HRA222 ASA GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. Use for exterior/interior electrical applications requiring UV resistance. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY HRA222 ASA (Asia Pacific) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. Use for exterior/interior electrical applications requiring UV resistance. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | ASTM D638 |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Asia Pacific) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Tensile Modulus | 2.52 GPa @Temperature 23.0 °C |
365 ksi @Temperature 73.4 °F |
Yield; ASTM D638 |
PolyOne Geon™ CPVC MC550 Polyvinyl Chloride, Chlorinated (CPVC) Information provided by PolyOne |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP GX07409H PSU LNP* LUBRICOMP* GX07409H is a compound based on PSU resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Healthcare. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp GX07409X PSU Wear resistant PSUThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP NX07354P PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating performance, a good candidate for Laser Direct Structuring applications. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Asia Pacific) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Tensile Modulus | 2.52 GPa | 365 ksi | ASTM D-638 |
Axiall 9113 Rigid PVC, Molding Georgia Gulf 9113 is used for a variety of packages including charcoal lighter fluid, toiletries and household chemicals. It has excellent impact strength.Information provided by Georgia GulfGeorgi.. |