Polymer Property : Tensile Modulus = 2.758 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.758 GPa
400.0 ksi
ASTM D638
Resirene Resirene® HH-107 General Purpose Polystyrene
Features:Medium FlowHigh HeatHigh Molecular WeightHigh ProductivityFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Thin Wall ApplicationsExtrusionGPPS/HIPS BlendsCD CasesCassette CasesInf..