Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 78761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87564 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M4300 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
PolyOne Nymax™ 1200 A Black 11 A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific) LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PS-15GB/15T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Nilit Polynil® P50FI Internally Lubricated Nylon 66 Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/5T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU) Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product .. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY SLDM2005 PC (Asia Pacific) Antistatic Polycarbonate, Non Halogen FR V-2 grade, mineral 5% filled |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Westlake Plastics Pomalux® Acetal Copolymer Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | |
Formosa Plastics Formolon® AW04 Homopolymer/Compound Homopolymer/Compound Formolon (AW04) is a NSF approved medium molecular weight dry blend PVC compound. This compound has been engineered primarily for rigid extrusion applications. The exceptional .. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Ensinger Tecatron® XP-72 Compression Molded PPS Compound, 20% PTFE Filled Natural Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D638 |
Ensinger PVC Polyvinylchloride (PVC) Ensinger's type 1 grey PVC ROD is designed for machining solutions and is a cost effective solution for general industrial applications. The material offers an excellent combination of chemical resi.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall 9275J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9275J Clear 38 is a food grade used for injection blow molded packages in critical medical, cosmetic and toiletry applications. All ingredients are FDA approved.Information provided by.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall HR-5009 Rigid PVC, Molding Georgia Gulf HR-5009 is a rigid, fitting-grade PVC compound designed for hot runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which incl.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall 8266 Natural 02 Rigid PVC, Extrusion, Natural 02 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Modulus | 2.83 GPa | 411 ksi | ASTM D638 |
Bayshore Vinyl Compounds BRC R409006/HR.WHT Injection Molding Compound BRC R409006/HR is a Type 1 / Grade 1 injection molding compound developed for hot runner applications. BRC R409006/HR meets the cell classification of 12454-B. BRC R409006/HR WHT has been designed.. |
|||
Tensile Modulus | 2.83 GPa | 410 ksi | ASTM D-638 |
Axiall 2503 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |