Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.5 GPa | 2100 ksi | |
Plastcom SLOVAMID 6 GF 50 TS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | |
Plastcom SLOVAMID 6 NG GF 45 SGF PA6, improved strength, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 45 % of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goo.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-2 |
PolyOne OnForce™ LFT NN-50LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-2 |
PolyOne OnForce™ LFT NY-50LGF/001 HS Natural Polyamide 6 (Nylon 6) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Therma-Tech™ NNC-5000 TC Polyamide 66 (Nylon 66) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)
(Unverified Data**) Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ASTM D638 |
PolyOne Edgetek® LCP-30GF/000 Liquid Crystal Polymer - 30% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1/-2 |
DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1,-2 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Tensile Modulus | 14.5 GPa @Temperature 23.0 °C |
2100 ksi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI LNP* STAT-KON* EE004 is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9X94104 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* 9X94104 is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1/-2 |
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50 Product Description: Grilamid 1SVX-50H black 9288 is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile. Key properties of Grilamid 1SBVX-50H LDS .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-4H1 black 9205 PA6T/6I-GF40 Product description: Grivory HTV-4H1 black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40 Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-4H black 9915 PA*-GF40 Product description: Grivory GV-6H EF natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50 Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA black 9225 is a 40 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Tensile Modulus | 14.5 GPa | 2100 ksi | ISO 527-1 |
Barlog Plastics KEBAFLOW MF130 LCP, 30% glass fiber reinforced LCP-GF30Information provided by BARLOG plastics GmbH. |